HY-208# silicone rubber mainly used for shoe molds, sand casting, sole sampling, plaster models, simple products, products with non-complex patterns, as well as product models with stable size and non-deformation.
Standard Datasheet:
Model : 208
Appearance : White
Viscosity (cs):15000
Hardness (A°): 30~35
Tensile Strength (kgf/c) ≥15
Tear Strength (kgf/) : ≥7.5
Elongation (%) : ≥200
Mixing ratio (%) : 2~3
Operating Time(h) : 0.5
Curing Time(h): 2~4
Model: 218#
Appearance: white
Viscosity (cs):7000
Hardness (A0): 10-20
Tensile Strength (kgf/c): ≥15
Tear Strength (kgf/): ≥7.5
Elongation (%):≥200
Mixing ratio (%): 2~3
Operating Time(h) : 0.5
Curing Time(h): 2~4
Using Instruction:
Component A is white flowing liquid and component B is the curing agent. For example, take silicone rubber of 100g and add 2% curing agent for mixing evenly. After the silicone rubber and the curing agent are completely mixed, put the silicon into a vacuum machine for deairing to remove the bubbles. After deaired, pouring the liquid silicone rubber into the product to be duplicated or into the mold frame.
Note: the product is used for pouring or brushing technique. That is to say, fix the product or sole model to be duplicated onto a plane plate, then enclose the plane frame with wooden plates to prevent the leakage of the silicon , mix the silicone rubber and the curing agent evenly according to the mixing ratio of 100 : 2 and pour them onto the sole model, then brush evenly with a wooden plate or a brush, and fill up the mold frame with gypsum after the silicone rubber is dried.